Dont you have a queen in canada? Your political voice in the USA is mute. If you wont post in other forums out of fear then pull out and dont lurk. The idea of your ideas getting squashed is bad it could be for several reasons that I wont mention ...
Hey Brian, was going to post this question, but tell me what you think: Lately some of the slabs I've been wet casting has not turned out like my sample. Tried to keep my ratios consistent and all, but I'm getting a lot of crumbly corners. I wait for 4 days before I unmold, but the corners are breaking off when I grind.
I use basic Quickrete sacks, BORG acrylic admix, and I keep the admix ratio pretty high (>50% volume). My mix is runny oatmeal consistency, in fact, when I level out the mold, there is a bit of water that comes to the top. Am I just not waiting long enough to work it? Thanks.